ナイロンの強靭化、押出機のL/D比に40:1を選ぶ理由

The third factor of nylon toughening – the determination of the production process, that the nylon toughening modification, it is usually used twin-screw blending modification, that twin-screw blending modification of course involves a twin-screw extruder, then how do we know and understand the twin-screw extruder it.



イメージ

Twin-screw extruder torque level

Generally speaking, the higher the torque rating, the better it is for modification.

When the output torque of the two screws is higher, the amount of material passed per unit time will be higher, which means that the more material passed per unit time, the lower the parallel shear rate will be.

That achieve the same plasticization effect, it will be less damage to the performance, so the same this case, the nylon made in the toughened material, the final performance is better.


Length to diameter ratio of twin-screw extruder

As for the aspect ratio, I think the aspect ratio suitable for nylon toughening can be 40:1, 44:1, or 48:1, in fact, we don’t need to care too much about the length of the aspect ratio. A proper 40:1 or more is enough for us to arrange our screw combination.

When the aspect ratio is longer, it has a longer residence time, but we can also adjust the screw combination to make it more dispersion of shear, in fact, it is also more conducive to the final effect of a modified nylon toughening.

新しい 記事

ナイロン強靭性向上のための適切なPOEグラフト無水マレイン酸の選び方とは?

補強と充填を必要とするPA6、PA66、ポリアミド系用の耐衝撃性改良剤として特別に設計されたCoace® W1A-Fは、その特殊な特性により、耐衝撃性と靭性の強化が最も重要な用途に最適です。

もっと読む→→→。

PBT改質における新たなブレークスルー:POE-g-GMA強化剤の画期的な応用

PBT改質におけるPOE-g-GMA強靭化剤の使用は、PBT材料の脆性に対処するだけでなく、プラスチック産業の新たな発展方向を提供する。

もっと読む→→→。

PP/PE複合材料にフィラーを加える場合、相溶化剤を加える必要がありますか?

PP-g-MAH相溶化剤の使用法を調べたい場合は、専門の化学品サプライヤーと連絡を取ることで、サンプルや技術サポートを得ることができる。COACEに相談することで、特定の用途のニーズを満たすためにミックスをカスタマイズすることができます。

もっと読む→→→。

メッセージを残す