Description des produits
The EPDM-g-MAH Aging Resistance A state-of-the-art product that provides remarkable performance in strengthening the aging resistance and cold resistance capabilities of EPDM and nylon materials is called Cold Resistance Super Tough Nylon Toughening Compatibilizer. This compatibilizer is made particularly to increase the compatibility between nylon and EPDM, creating a material that is robust, long-lasting, and better able to withstand aging and low temperatures. This product is redefining the market with its distinctive formulation and cutting-edge technology by offering improved performance and dependability across a range of applications.
Enhancing the age resistance and cold resistance capabilities of EPDM and nylon materials is the main goal of the age Resistance EPDM-g-MAH Cold Resistance Super Tough Nylon Toughening Compatibilizer. By serving as a link between the two components, this compatibilizer increases their compatibility and produces a synergistic result. It successfully stops EPDM and nylon from deteriorating from age and exposure to cold temperatures, assuring the life and durability of the finished product. This compatibilizer also improves the material’s strength and toughness, making it ideal for demanding applications.
Un équipement de pointe !
Elle est équipée de lignes de production avancées et d'un centre d'essais expérimentaux pour garantir la qualité des produits.
Une force technique puissante !
Plus de 10 techniciens expérimentés en recherche et développement sont à l'origine d'une innovation permanente.
Table1: Typical Data of Toughening of PA6 Resin
Performance | Unité | PA6 | PA6+15%W1P | PA6+20%W1P |
Résistance à la traction | MPa | 60 | 55 | 50 |
Résistance à la flexion | MPa | 90 | 80 | 70 |
Résistance à l'impact de l'entaille de Lzod (23℃) | J/m | 80 | 700 | 1000 |
Table2: Typical Data of Toughening of PA66 Resin
Performance | Unité | PA66 | PA66+15%W1P | PA66+20%W1P |
Résistance à la traction | MPa | 75 | 57 | 55 |
Résistance à la flexion | MPa | 102 | 85 | 80 |
Résistance à l'impact de l'entaille de Lzod (23℃) | J/m | 80 | 800 | 1000 |
Dose suggérée: The dose (5–25%) may be appropriately raised or lowered in accordance with the demands for toughness and by taking the cost into account.While 5% must be used as a nylon and polypropylene/polyethylene alloy compatibilizer, 3-10% must be used to reinforce and toughen PA6/PA66.
Emballage, stockage et transport : Internal plastic bag in a 20 kilogram kraft bag. This product must be handled as a non-hazardous item, kept or transported in a dry environment, and sunshine and precipitation must be avoided.
Support A
Notre avantage
service complet !
Selection recommendation
Support technique
Protection après-vente
service complet !
Selection recommendation
Support technique
Protection après-vente
service complet !
Selection recommendation
Support technique
Protection après-vente
service complet !
Selection recommendation
Support technique
Protection après-vente
fter-sales protection
Caractéristique
This product, which is an ethylene-propylene-diene monomer with functionalized maleic anhydride, is best suited for nylon that is extremely durable or cold-resistant.
Élément de test | Données d'essai | Méthode d'essai |
densité | 0,87 g/cm³ | ASTM D792 ISO 1183 |
Indice de fusion | 0.1-0.4(190℃,2.16kg)g/10min | ASTM D1238 ISO 1133 |
Greffe | Haut | taux de titrage acide-base |
Remarque :Les données sont dérivées de la valeur moyenne de l'échantillon de rétention du produit testé dans les six mois, et ces données sont mises à jour tous les six mois. Taux de greffe standard : faible<0,4% ; moyen 0,4%-0,8% ; élevé ≥0,8%
Avantage
1. Aging Resistance: EPDM-g-MAH for Aging Resistance With its remarkable aging resistance qualities, Cold Resistance Super Tough Nylon Toughening Compatibilizer ensures that the material will stay dependable and durable even under challenging climatic circumstances. The lifespan of the material is extended because it successfully delays deterioration and degradation brought on by exposure to UV light, heat, and other aging causes.
2. Cold Resistance: This compatibilizer was especially created to improve the EPDM and nylon materials’ capacity to withstand cold temperatures. It makes it possible for the material to keep its flexibility and toughness even at low temperatures, making it suited for use in areas with frequent temperature variations or in cold climes.
3. Toughening: By adding this compatibilizer, nylon and EPDM materials are both much more resilient. It increases the material’s tensile strength, tear resistance, and impact resistance, enabling it to be used in demanding applications that need a high level of toughness and durability.
4. Compatibility: By successfully enhancing the compatibility between EPDM and nylon, the Aging Resistance EPDM-g-MAH Cold Resistance Super Tough Nylon Toughening Compatibilizer ensures improved dispersion and adhesion between the two materials. A more uniform and homogenous material with enhanced mechanical qualities is produced as a result of the compatibility improvement.
Notre avantage
Chaîne d'approvisionnement mondiale !
Sound Storage And Logistics Supply Chain System (système de chaîne d'approvisionnement)
Support technique
Protection après-vente
Concentration - Réalisation - Excellence !
Produits personnalisés
Priorité à la R&D
Services globaux
Certification Coace !
Certification ISO9001:2015
Certification ISO14001:2015
Enregistrement REACH dans l'UE
Corée K-REACH pré-enregistrement
L'avantage de l'entreprise !
Disposition à l'intérieur et à l'extérieur du pays, idéal pour les mélanges
Schéma de commercialisation intérieure
Mise en place d'un marketing outre-mer
Application
W1P can be used for PA6 PA66 or PP super-tough.Increase the ultra-cold impact resistance and processability of material , decrease the water absorption,and greatly improve the cold resistance.
It can be used for the compatibilizer of nylon and polypropylene alloy.